Water Based without Flash

Posted: Thu Oct 30, 2014 6:36 am
by kajun1950
I do not have a flash dryer or conveyor, just a heat gun. Other than screen clogging what is benefit of water base over plastisol.

Re: Water Based without Flash

Posted: Thu Oct 30, 2014 8:23 pm
by Catspit Productions
The only benefit in my opinion is the feel of the print. Others will say it is more environmental. Water based is more difficult to print with than plastisol. As a result it is easier to learn with plastisol.

http://www.catspitproductionsllc.com/intro-to-inks.html

http://www.catspitproductionsllc.com/wa ... dinks.html

Those articles should help.

Re: Water Based without Flash

Posted: Thu Oct 30, 2014 10:45 pm
by kajun1950
I have a swing-a-way heat press, could I use this for a dryer? Maybe with Teflon sheet and no pressure just lowered onto garment

Re: Water Based without Flash

Posted: Mon Nov 03, 2014 8:47 am
by Catspit Productions
It's possible but will require some testing to iron out your process. Many people use heat presses to cure inks in different ways. I did an experiment with it and found that with light pressure and a Teflon sheet it can be done. I never tried to just lower the heating element however. Since the radiant heat from the heat press is minimal I figured it would take too long to be practical but who knows.


Re: Water Based without Flash

Posted: Mon Nov 03, 2014 8:54 am
by kajun1950
Thanks, I will play with soon and see.

John